Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 2RE69 is a fully austenitic stainless steel with extra low carbon and impurity contents. The grade is characterized by:

  • Excellent resistance to corrosion in ammonium carbamate and nitric acid
  • Excellent resistance to intergranular corrosion
  • High resistance to pitting and crevice corrosion
  • Good weldability

Sandvik 2RE69 has been developed primarily to cope with the severe corrosive conditions existing in the urea industry. The longest service life is so far 35 years, which confirms the optimal properties for the grade Sandvik 2RE69 in urea strippers.

Standards

  • UNS: S31050
  • EN Number: 1.4466
  • EN Name: X1CrNiMoN25-22-2
  • W.Nr.: 1.4466* 1), 1.4465* 2)
  • DIN: X 2 CrNiMo 25 22 2* 1), X 1/CrNiMoN 25 25 2* 2)
  • AFNOR: Z 1 CND25.22AZ

* Obsolete. Replaced by EN.

1) Appearing in TÜV Wien-Werkstoffblatt 093
2) Appearing in SEW400

Urea specifications issued by:

  • Stamicarbon
  • Saipem
  • Kellogg
  • Urea Casale

Product standards

  • ASTM A213, A312
  • EN 10216-5
  • SEW 400

Approvals

  • Approved by the American Society of Mechanical Engineers (ASME) for use in accordance with ASME Boiler and Pressure Vessel Code, Section VIII, Divisions 1 and 2
  • ASME Code Case 2038-5 for forgings
  • TÜV Wien-Werkstoffblatt 093

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.