Sandvik 3R12

Tube and pipe, seamlessDatasheet

Datasheet updated 2020-12-10 06:47 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 3R12 is an austenitic stainless chromium-nickel steel with a low carbon content.

Standards

  • ASTM: TP304L, TP304
  • UNS: S30403, S30400
  • EN Number: 1.4306, 1.4301
  • W.Nr.: 1.4306*, 1.4301*
  • DIN: X 2 CrNi 19 11*, X 5 CrNi 18 10*
  • SS: 2352*, 2333*
  • AFNOR: Z 2 CN 18.10*
  • BS: 304S31*, 304S11*
  • JIS: SUS304L, SUS304LTB, SUS304TP

Product standards

  • ASTM A213, A269 and A312
  • JIS G3459
  • JIS G3463
  • EN 10216-5
  • BS 3605, 3606*
  • DIN 17456, 17458*
  • NFA 49-117, 49-217
  • SS 14 23 52, 14 23 33*

* Obsolete. Replaced by EN.

Approval
JIS approval for Stainless Steel Tubes

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.