Sandvik 3R19 is an austenitic stainless steel with low carbon content alloyed with nitrogen.
Standards
-
ASTM: TP304LN -
UNS: S30453 -
EN Number: 1.4311 -
W.Nr.: 1.4311* -
DIN: X 2 CrNiN 18 10* -
SS: 2371* -
AFNOR: Z2CN18-10Az*
* Obsolete. Replaced by EN.
Chemical composition (nominal)
C | Si | Mn | P | S | Cr | Ni |
---|---|---|---|---|---|---|
≤0.030 | 0.4 | 1.3 | ≤0.040 | ≤0.030 | 18.5 | 9 |
Others
N=0.14
Mechanical properties
Proof strength | Tensile strength | Elong. |
---|---|---|
Rp0.2a) | Rm | Ab) |
MPa | MPa | % |
≥270 | 550-750 | ≥35 |
1 MPa = 1 N/mm2
a) Rp0.2 and Rp1.0 correspond to 0.2% offset and 1.0% offset yield strength, respectively.
b) Based on L0 = 5.65 √S0 where L0 is the original gauge length and S0 the original cross-section.
Proof strength | Tensile strength | Elong. |
---|---|---|
Rp0.2a) | Rm | Ab) |
ksi | ksi | % |
≥39 | ≥80-109 | ≥35 |
a) Rp0.2 and Rp1.0 correspond to 0.2% offset and 1.0% offset yield strength, respectively.
b) Based on L0 = 5.65 √S0 where L0 is the original gauge length and S0 the original cross-section.