Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 6R35 is an austenitic, titanium-stabilized stainless chromium-nickel steel. It is suitable for wet-corrosive service but also has good mechanical strength at high temperatures.

Standards

  • ASTM: TP321, TP321H
  • UNS: S32100, S32109
  • EN Number: 1.4541, 1.4940
  • EN Name: X6CrNiTi18-10, X7CrNiTi18-10
  • W.Nr.: 1.4541, 1.4878
  • DIN: X6CrNiTi 18 10, X12CrNiTi 18 9
  • SS: 2337
  • AFNOR: Z6CNT18-10
  • BS: 321S31, 321S51

Product standards

Seamless tube and pipe

  • ASTM A213, A312, A269, A376, (A511)
  • EN 10216-5
  • BS 3059, 3605, 3606
  • DIN 17456, 17458
  • SS 14 23 37
  • NFA 49-117, 49-217

Approvals

PED (Pressure Equipment Directive) 2014/68/EU and AD2000

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.