Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sanicro® 30 is a low-carbon version of Alloy 800 austenitic nickel-iron-chromium alloy. The grade is used for steam generator tubing in nuclear stations (PWR) and other heat exchangers for temperature up to about 550°C (1020°F) where good resistance to stress corrosion cracking (SCC) and intergranular corrosion is required.

Standards

  • UNS: N08800
  • EN Number: 1.4558
  • EN Name: X2NiCrAlTi32-20
  • W.Nr.: 1.4558
  • DIN: X 2 NiCrAlTi 32 20
  • BS: NA15

Product standards
Seamless condenser and heat exchanger tubes: ASTM A213, B163, EN 10216-5

Seamless tube and pipe: ASTM A312, B407, EN 10216-5

Approvals
Approved for use according to ASME Boiler and Pressure Vessel Code Section III, division 1 and Section VIII, division 1 and 2

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.