Bridas ciegas inoxidables de 600 lb

ASTM A182, ASME B16.5
Superficie elevada, acabado liso (125-250 RMS / 3,2-6,3 µm)
Ejemplo de código de producto:
FFB-304L-2-600
Tubería | Brida | Superficie elevada | Plantilla de taladrado | Peso | Existencias estándar | |||||
---|---|---|---|---|---|---|---|---|---|---|
Tamaño nominal | OD1 | D | b | g | l | k | Nº. de orificios | kg/pieza | ASTM 304L | ASTM 316L |
pulg. | mm | mm | mm | mm | mm | mm | ||||
1/2 3/4 1 1 ½ |
21.3
26.7 33.4 48.3 |
95.2
117.5 124.0 155.4 |
14.3
15.9 17.5 22.4 |
34.9
42.9 50.8 73.2 |
15.9
19.0 19.1 22.4 |
66.7
82.5 88.9 114.3 |
4
4 4 4 |
0.700
1.200 1.600 3.250 |
●
● - - |
●
● ● ● |
2 3 4 6 |
60.3
88.9 114.3 168.3 |
165.1
209.6 273.1 355.6 |
25.4
31.8 38.1 47.8 |
91.9
127.0 157.2 215.9 |
19.1
22.4 25.4 28.4 |
127.0
168.1 215.9 292.1 |
8
8 8 12 |
4.150
8.440 17.300 36.100 |
●
● ● ● |
●
● ● - |
1 OD = diámetro exterior