Bridas de uniones traslapadas inoxidables de 150 lb

ASTM A182, ASME B16.5
Superficie plana, acabado liso (125-250 RMS/3,2-6,3 µm)
Ejemplo de código de producto:
FFLJ-316L-2-150
● = existencias estándar
Tubería | Brida | Cubo | Plantilla de taladrado | Peso | Existencias estándar | |||||||
---|---|---|---|---|---|---|---|---|---|---|---|---|
Tamaño nominal | OD1 | D | J | b | h | r | m | l | k | Nº. de orificios | kg/pieza | ASTM 316L |
pulg. | mm | mm | mm | mm | mm | mm | mm | mm | mm | |||
1/2 3/4 1 1 ½ |
21.3
26.7 33.4 48.3 |
88.9
98.6 108.0 127.0 |
22.9
28.2 35.1 50.0 |
11.2
12.7 14.2 17.5 |
15.7
15.7 17.5 22.4 |
3.0
3.0 3.0 6.4 |
30.2
38.1 49.3 65.0 |
15.7
15.7 15.7 15.7 |
60.5
69.9 79.2 98.6 |
4
4 4 4 |
0.390
0.560 0.780 1.320 |
●
● ● ● |
2 3 4 6 |
60.3
88.9 114.3 168.3 |
152.4
190.5 228.6 279.6 |
62.5
91.4 116.8 171.5 |
19.1
23.9 23.9 25.4 |
25.4
30.2 33.3 39.6 |
7.9
9.7 11.2 12.7 |
77.7
108.0 134.9 192.0 |
19.1
19.1 19.1 22.4 |
120.7
152.4 190.5 241.3 |
4
4 8 8 |
2.060
3.850 5.300 7.450 |
●
● ● ● |
1 OD = diámetro exterior