Bridas deslizantes inoxidables de 300 lb

ASTM A182, ASME B16.5
Superficie elevada, acabado liso (125-250 RMS / 3,2-6,3 µm)
Ejemplo de código de producto:
FFSO-304L-2-300
Tubería | Brida | Cubo | Superficie elevada | Plantilla de taladrado | Peso | Existencias estándar | |||||||
---|---|---|---|---|---|---|---|---|---|---|---|---|---|
Tamaño nominal |
OD1 | D | J | b | h | m | g | l | k | Nº. de orificios |
kg/pieza | ASTM 304L |
ASTM 316L |
pulg. | mm | mm | mm | mm | mm | mm | mm | mm | mm | ||||
1/2 3/4 1 1 ¼ |
21.3
26.7 33.4 42.2 |
95.3
117.3 123.9 133.3 |
22.3
27.7 34.5 43.2 |
14.2
15.7 17.5 19.0 |
22.3
25.4 26.9 27.0 |
38.1
47.7 53.8 63.5 |
35.0
42.9 50.8 63.5 |
15.7
19.0 19.0 19.0 |
66.5
82.5 88.9 98.4 |
4
4 4 4 |
0.640
1.120 1.360 1.800 |
●
● ● ● |
●
● ● ● |
1 ½ 2 2 ½ 3 |
48.3
60.3 73.0 88.9 |
155.4
165.1 190.5 209.5 |
49.5
62.0 74.7 90.7 |
20.6
22.3 25.4 28.4 |
30.2
33.2 38.1 42.9 |
69.8
84.0 100.0 117.3 |
73.1
91.9 104.8 127.0 |
22.3
19.0 22.2 22.3 |
114.3
127.0 149.2 168.1 |
4
8 8 8 |
2.490
2.870 4.400 5.850 |
●
● ● ● |
●
● ● ● |
4 5 6 8 |
114.3
141.3 168.3 219.1 |
254.0
279.4 317.5 381.0 |
116.1
143.8 170.7 221.5 |
31.7
35.1 36.5 41.1 |
47.7
50.8 52.3 61.9 |
146.0
177.8 206.2 260.3 |
157.2
185.7 215.9 269.7 |
22.3
22.4 22.3 25.4 |
200.1
235.0 269.7 330.2 |
8
8 12 12 |
9.610
12.300 15.600 24.200 |
●
● ● |
●
● ● ● |
10 12 |
273.0
520.7 |
444.5
520.7 |
276.4
327.2 |
47.6
50.8 |
66.7
73.0 |
320.7
374.6 |
323.8
381.0 |
28.6
31.7 |
387.3
450.8 |
16
16 |
37.100
50.000 |
●
● |
●
● |
1 OD = diámetro exterior