Sandvik 6RA11

BilletsTietolomake

Aineslehti on päivitetty 2019-11-14 13.43 (tämä versio korvaa kaikki aiemmat versiot)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 6RA11 is an austenitic stainless free-machining steel with addition of sulphur.

Standards

  • ASTM: 303
  • UNS: S30300
  • EN Number: 1.4305
  • W.Nr.: 1.4305

Product standards

  • EN 10088-3
  • ASTM A-314

Certificates

Status according to EN 10 204 3.1

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Lähetä PDF-tiedosto sähköpostin liitteenä