Forging and re-rolling billets

Forging billets and re-rolling billets in a wide range of stainless steels, duplex stainless steels and nickel alloys. The billets are 100% ultrasonically and eddy current tested in a fully automated inspection line to ensure the highest quality standards.

View list of materials

Haluatko lisätietoja?

Soita Lähetä sähköpostia

Forging billets

Sandvik's billets for forging are suitable for producing all types of forged products, such as flanges, discs, rings, valves, forged parts, and axles. Our program of forging billets includes a wide range of stainless steels and high-alloy materials.

Re-rolling billets

Billets for re-rolling of strip, wire, bar, hexagons and profiles, available in square and rectangular sizes. The production route for re-rolling billets is often more simplified than that for forging billets, since in most cases products do not require a dense center. For many of these products, continuous cast material can be used, which contributes to lower raw material costs.

Standard program

Square billets
Size range,
mm (in.)
Tolerances,
mm (in.)
Lengths,
m (ft)
Surface condition
80 – 200
(3.15 – 7.87)
± 2 - ± 4
(±0.078 – ±0.157)
4 – 6.3
(13.1 – 20.7)
Black (unground)
Spot ground
Fully ground
>200 – 350
(>7.87 – 13.78)
±5 (±0.1968)
3 – 5.3
(9.8 – 17.4)
Fully ground
Round billets
Size range,
mm (in.)
Tolerances,
mm (in.)
Lengths,
m (ft)
Surface condition
80 – 200
(3.15 – 7.87)
±3 (± 0.118) max 10
(32.8)
Peel turned
>200 – 450
(>7.87 – 17.72)
±5 (±0.1968) 3 – 8
(9.8 – 26.2)
Peel turned
Rough turned
77 – 193
(3.03 – 7.60)
±2 (±0.078) max 10
(32.8)
Black (unground)
>200 – 450
(>7.87 – 17.72)
±5 (±0.1968) 3 – 8
(9.8 – 26.2)