Sandvik SAF 2507

Sandvik SAF 2507, also known as SAF 2507, is Sandvik's trademark for a super-duplex stainless steel characterized by excellent resistance to stress corrosion cracking (SCC), very high resistance to pitting and crevice corrosion, high resistance to general corrosion and very high mechanical strength.

Sandvik SAF 2507 super-duplex steel is available as tube and pipe, bar, billets and strip.

Sandvik 25.10.4.L welding wire and Sandvik 25.10.4.LR covered electrodes are specially developed welding consumables for Sandvik SAF 2507.

Material datasheets

Related datasheets

Prodotti correlati

Tube and pipe in seamless and welded condition, fittings and flanges.

Stainless round bar for machining

Forging billets, re-rolling billets, extrusion billets and continuous cast blooms.

Precision strip steel.

Slicklines and armor wire for logging cables in a wide range of stainless steels and high-alloyed materials.