Welded pipe in sizes according to ASTM/ASME

Stainless welded pipe in sizes according to ASTM/ASME. Pipe is supplied annealed and pickled in random lengths or cut to fixed lengths in steel grades ASTM 304L and 316L. Welded pipes are either 100% Eddy Current tested or hydrostatic and expansion tested.

Available online

This product can be ordered online via our self-service platform E-Track, where you can also see stocks, get prices and view your order history.

E-Track is currently available in selected European countries but we are working on expanding the availability.


ORDER IN E-TRACK


Stock program

Pipe is stocked according to ASTM A312/ASME SA 312, ASTM A999/M
Tolerances according to ASME B36.19.
OD = outside diameter, WT = wall thickness.

OD
mm
WT
mm
Nominal size Weight, kg/m 304L 316L
21.34 2.11 1/2" SCH 10S 1.02
21.34 2.77 1/2" SCH 40S 1.29
26.67 2.11 3/4" SCH 10S 1.30
26.67 2.87 3/4" SCH 40S 1.71
33.40 1.65 1" SCH 5S 1.31
33.40 2.77 1" SCH 10S 2.13
33.40 3.38 1" SCH 40S 2.54
42.16 1.65 1 1/4" SCH 5S 1.67
42.16 2.77 1 1/4" SCH 10S 2.73
42.16 3.56 1 1/4" SCH 40s 3.44
48.26 1.65 1 1/2" SCH 5S 1.92
48.26 2.77 1 1/2" SCH 10S 3.16
48.26 3.68 1 1/2" SCH 40S 5.49
60.33 1.65 2" SCH 5S 2.42
60.33 2.77 2" SCH 10S 3.99
60.33 3.91 2" SCH 40S 5.52
73 3.05 2 1/2" SCH 10s 5.35
73 5.16 2 1/2" SCH 40S 8.77
88.90 2.11 3" SCH 5S 4.58
88.90 3.05 3" SCH 10S 6.56
88.90 5.49 3" SCH 40S 11.47
101.60 3.05 3 1/2" SCH 10s 7.53
114.30 2.11 4" SCH 5S 5.93
114.30 3.05 4" SCH 10S 8.50
114.30 6.02 4" SCH 40S 16.32
141.3 3.4 5" SCH 10S 11.74
141.3 6.55 5" SCH 40S 22.1
168.3 2.77 6" SCH 5S 11.48
168.3 3.4 6" SCH 10S 14.04
168.3 7.11 6" SCH 40S 28.69
219.1 2.77 8" SCH 5S 15.0
219.1 3.76 8" SCH 10S 20.27
219.1 8.18 8" SCH 40S 43.2
273 3.40 10" SCH 5S 22.95
273 4.19 10" SCH 10S 28.2
273 9.27 10" SCH 40S 61.22
323.9 3.96 12" SCH 5S 31.72
323.9 4.57 12" SCH 10S 36.54
323.9 9.53 12" SCH 40S 75.02
355.6 4.78 14" SCH 10S 41.99
355.6 9.53 14" SCH STD 82.583
406.4 9.53 16" SCH STD 94.706
406.4 4.78 16" SCH 10S 48.07
457.2 4.78 18" SCH 10S 54.151
508.0 5.54 20" SCH 10S 69.702
610.0 6.35 *24" SCH 10S 95.919

*24" is produced with two seams