Sanicro® 75X

Strip steel데이터시트

데이터시트 업데이트됨 2020-12-10 07:47 (모든 이전 판 대체)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sanicro® 75X is a precipitation hardening nickel alloy with good spring properties and good resistance to gas corrosion at high temperatures. Due to the grade's low cobalt content, Sanicro® 75X is particularly suitable for nuclear power applications.

Standards

  • UNS: N07750

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.