Aqui você pode acessar os "datasheets" de nossa ampla gama de ligas e materiais. Contate-nos se você necessitar de mais informações sobre nossos materiais.
Standard:EN number 1.4369
An austenitic stainless steel combining high mechanical strength with a non-magnetic structure. The grade has good fatigue properties and excellent ductility and is typically used for springs and other high strength applications.
Standard:UNS S31673
A molybdenum-alloyed high-strength vacuum remelted austenitic stainless steel with excellent microcleanliness and structural homogeneity. The grade is part of the Sandvik medical materials range.
Standard:UNS S30400, S30409 | ASTM TP304, TP304H | EN number 1.4301, 1.4948
An austenitic stainless steel with controlled carbon content for improved strength at high temperatures.
Standard:UNS S30453 | ASTM TP304LN | EN number 1.4311
An austenitic stainless steel with low carbon content alloyed with nitrogen.
Standard:UNS R52400 | ASTM Grade 7
An unalloyed titanium grade with standard oxygen content and addition of palladium (0.12–0.25%).
Standard:UNS R 60702
A zirconium grade characterized by immunity to stress corrosion cracking and high resistance to pitting and crevice corrosion. The grade has very good corrosion resistance in, for example, several types of acids and moderate mechanical strength.
Standard:UNS R52402 | ASTM Grade 16
An unalloyed titanium grade with standard oxygen content and addition of palladium (0.04–0.08%).
Standard:UNS N06690
An austenitic nickel-chromium-iron (NiCrFe) alloy used primarily for steam generators in nuclear power plants (PWR). The grade is also suitable for use in caustic environments and nitric acid.
Standard:UNS S31635 | ASTM 316Ti | EN number 1.4571
A titanium-stabilized, molybdenum-alloyed austenitic stainless steel with improved machinability.
Standard:UNS N08029 | ASTM B668-05
Sanicro® 29 is a high-alloy austenitic stainless steel for service in highly corrosive conditions. Sanicro® 29 was originally developed as an alternative to Sanicro® 28, with improved localized corrosion resistance where the environment contains high chloride concentrations. With the addition of molybdenum the PRE (Pitting Resistance Equivalent) has been increased from ≥38 for Sanicro® 28, to ≥42.