Standard:
Bond CJL is a high temperature thermoplastic polyester bondcoat, that exhibits good bond strength after activation with heat at 170-190°C. Bond CJL can also be activated with solvent. This allows windings that maintain their shape until permanently bonded with heat. The recommended solvents for activation of this material are acetone or methyl ethyl ketone.
Standard:UNS N08935
Sanicro® 35 is an alloy combining the best features of a super austenitic stainless steel and a nickel alloy. The grade has excellent corrosion resistance, for service in sea-water applications and other highly corrosive environments.
Sanbar® 23 is an air-hardening, high chromium-molybdenum alloy steel with good response to surface induction hardening and suitable for carburizing. It has high fatigue strength and wear resistance in the case hardened condition.
Sanbar® 61 is a high strength silicon steel with good toughness and impact resistance in the as-rolled condition.
Um esmalte é fabricado a partir de resinas de acetal de vinil.
Um esmalte de fio de poliimida classe 240, tipo 1 modificado.
Um revestimento aderente de epóxi com modificação termoplástica.
Um revestimento de fluoropolímero sintético.
Standard:UNS N08825 | EN number 2.4858
Sanicro® 825 is a nickel alloy with high iron content and a copper addition, suitable for applications in special corrosive environments.
Sanbar® 64 is an air-hardening, high nickel alloy steel with good response to carburizing. It has excellent fatigue strength and wear resistance in the case hardened condition.