Aqui você pode acessar os "datasheets" de nossa ampla gama de ligas e materiais. Contate-nos se você necessitar de mais informações sobre nossos materiais.
Standard:UNS N08825 | EN number 2.4858
Sanicro® 825 is a nickel alloy with high iron content and a copper addition, suitable for applications in special corrosive environments.
Standard:
Sanbar® 64 is an air-hardening, high nickel alloy steel with good response to carburizing. It has excellent fatigue strength and wear resistance in the case hardened condition.
Standard:UNS S31603, S31600 | ASTM 316L, 316 | EN number 1.4435, 1.4436
A molybdenum-alloyed (min. 2.5% Mo) austenitic stainless steel with improved machinability.
Standard:UNS S31600, S31603 | ASTM 316, 316L | EN number 1.4401, 1.4404
A molybdenum-alloyed austenitic stainless steel with improved machinability.
A hardenable, free-cutting carbon steel characterized by excellent machinability. It has high hardness, high wear resistance and exceptional dimensional stability after hardening. The grade is part of the Sandvik Exera® medical materials range.
Standard:UNS S46910
A precipitation hardening stainless steel specifically designed for applications requiring high strength combined with good ductility in the final product. The grade has a good tempering effect and is part of the Exera® medical materials range.
Standard:ASTM F562-02
Cobalt-chromium-molybdenum (CoCrMo) alloys with high tensile strength, excellent corrosion properties and good ductility. The alloys are part of the Exera® medical materials range.
Wire with polymer coatings and metallic electroplating.
Standard:ASTM 420 | EN number 1.4028 Mod./1.4031 Mod.
A martensitic stainless chromium steel with very good formability that after hardening and tempering is characterized by high corrosion resistance and toughness. The grade is part of the Exera® medical materials range.
View datasheet for:
UNS S30815 | ASTM F45 | EN number 1.4835
An austenitic chromium-nickel steel alloyed with nitrogen and rare earth metals for high-temperature applications. Sandvik 253 MA is characterized by high creep strength, very good resistance to isothermal and cyclic oxidation.
Several product forms available: