Aqui você pode acessar os "datasheets" de nossa ampla gama de ligas e materiais. Contate-nos se você necessitar de mais informações sobre nossos materiais.
View datasheet for:
UNS N06600
An austenitic nickel-chromium-iron alloy characterized by very good resistance to carburization and nitrogen absorption and good structural stability at high temperatures. It has also good resistance to stress corrosion cracking.
Several product forms available:
Standard:
We offer a variety of polyimide coatings that can be applied to all our alloy offerings. Polyimides are chosen in applications because of their excellent resistance to chemicals, superior abrasion resistance, and superior thermal performance. Because of this combination of features, they are typically chosen for use in the most rigorous of applications.
Uma resina de poliéster modificada com sobrecamada adicional de Nylon.
Um revestimento de etileno propileno fluorado.
Standard:UNS S31600/ S31603 | ASTM 316/316L | EN number 1.4401/1.4404
Austenitic stainless steel alloyed with molybdenum. The grades are part of the Exera® medical materials range.
UNS S31600, S31603 | ASTM 316, 316L, MT 316, MT 316L | EN number 1.4435, 1.4436
A molybdenum-alloyed (min. 2.5% Mo) austenitic stainless steel with improved machinability.
UNS S31635 | ASTM 316 Ti, 316Ti | EN number 1.4571
A titanium-stabilized, molybdenum-alloyed austenitic stainless steel with improved machinability.
UNS S31600, S31609 | ASTM 316, 316H, TP316, TP316H | EN number 1.4401
A molybdenum-alloyed austenitic stainless steel.
Standard:UNS S30403 | ASTM 304L | EN number 1.4301/1.4307
An austenitic stainless steel with a low carbon content.
Standard:UNS S31703 | ASTM 317L | EN number 1.4438
An austenitic stainless steel with a high molybdenum content. The grade is characterized by improved resistance to general and pitting corrosion in comparison with ASTM 316L.
Go to page: Previous , 1 , … , 3 , 4 , 5 , 6(This page) , 7 , 8 , 9 , … , 20 Next