Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sanicro® 28 is a high-alloy multi-purpose austenitic stainless steel for service in highly corrosive conditions. The grade is characterized by:

  • Very high corrosion resistance in strong acids
  • Very good resistance to stress corrosion cracking (SCC) and intergranular corrosion in various environments
  • High resistance to pitting and crevice corrosion
  • Good weldability

Standards

  • UNS: N08028
  • EN Number: 1.4563
  • EN Name: X 1 NiCrMoCu 31-27-4
  • W.Nr.: 1.4563

Standards

Product standard
EN 10088-3, EN 10272
Certificates
Status according to EN 10 204 3.1

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.