Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

SAF 2507® is a high alloy super duplex (austenitic-ferritic) stainless steel for service in highly corrosive conditions. The grade is characterized by:

  • Excellent resistance to stress corrosion cracking in chloride-bearing environments
  • Excellent resistance to pitting and crevice corrosion
  • High resistance to general corrosion
  • Very high mechanical strength
  • Physical properties that offer design advantages
  • High resistance to erosion corrosion and corrosion fatigue
  • Good weldability

Standards

  • UNS: S32750
  • EN Number: 1.4410
  • EN Name: X 2 CrNiMoN 25-7-4

Product standards

  • EN 10216-5
  • EN 10297-2
  • ASTM A511, A790
  • NORSOK MDS D51

Approvals

  • Pressure Equipment Directive (2014/68/EU)
  • Approved by the American Society of Mechanical Engineers (ASME) for use in accordance with ASME Boiler and Pressure Vessel Code, Section VIII, div. 1
  • ASME B31.3 Chemical Plant and Petroleum Refinery piping
  • VdTÜV-Werkstoffblatt 508
  • ISO 15156-3/NACE MR 0175 (Sulphide stress cracking resistant material for oil field equipment). Applies to liquid quenched tubes

Certificate

Status according to EN 10 204/3.1

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.