Sanmac® 316/316L

Hollow barDatasheet

Datasheet updated 2020-12-10 07:47 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sanmac® 316/316L is a molybdenum-alloyed austenitic chromium-nickel steel with improved machinability.

Standards

  • ASTM: MT 316, MT 316L
  • UNS: S31600, S31603
  • EN Number: 1.4401, 1.4404
  • EN Name: X 5 CrNiMo 17-12-2, X 2 CrNiMo 17-12-2
  • JIS: SUS316TKA

Product standards

  • EN 10216-5*, EN 10297-2, EN 10294-2
  • ASTM A511
  • JIS G3446

* The leakage test is deferred to the finished component

Approval
JIS Approval No. SE9402 for Stainless Steel Tubes

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.