SAF 2507®

BilletsDatasheet

Datasheet updated 2021-09-30 05:25 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

SAF 2507® is a super-duplex (austenitic-ferritic) stainless steel for service in highly corrosive conditions. The grade is characterized by:

  • Excellent resistance to stress corrosion cracking (SCC) in chloride-bearing environments
  • Excellent resistance to pitting and crevice corrosion
  • High resistance to general corrosion
  • Very high mechanical strength
  • Physical properties that offer design advantages
  • High resistance to erosion corrosion and corrosion fatigue
  • Good weldability

Standards

  • UNS: S32750
  • EN Number: 1.4410
  • EN Name: X 2 CrNiMoN 25-7-4
  • SS: 2328

Product standards

EN 10088-3
Suitable for further production according to ASTM A182 Grade F53.
Chemical composition according to ASTM A479, UNS S32750

Certificates

Status according to EN 10 204 3.1

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.