Sanicro® 31HT

BilletsDatasheet

Datasheet updated 2020-12-10 06:47 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sanicro® 31HT, commonly known as Alloy 800HT, is an austenitic nickel-iron-chromium alloy. It is characterized by:

  • High creep strength
  • Very good resistance to oxidation
  • Good resistance to combustion gases
  • Very good resistance to carburization
  • Good resistance to nitrogen absorption
  • Good structural stability at high temperatures
  • Good weldability

The grade can be used at temperatures up to about 1100°C (2010°F). In order to have the best ductility this grade should be used above 700°C (1290°F). Because of its high nickel content and prescribed maximization of (Ti + Al) content, Sanicro® 31HT shows extremely little tendency to precipitation of embrittling phases.

Standards

  • UNS: N08810/N08811
  • EN Number: 1.4959
  • W.Nr.: 1.4876/1.4959

Product Standards

Suitable for the production of flanges etc. according to ASTM B564
Chemical composition according to EN 10095.

Certificate

Status according to EN 10 204/3.1

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.