SAF 2906™

Tube and pipe, seamlessDatasheet

Datasheet updated 2021-03-05 17:14 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

SAF 2906™ is a high-alloy duplex (austenitic-ferritic) stainless steel with excellent corrosion resistance in caustic environments and environments with chlorides. SAF 2906™ characteristics:

  • Excellent resistance to caustic environments, also in the presence of contaminants such as chlorides
  • Excellent resistance to intergranular corrosion
  • Excellent resistance to pitting and crevice corrosion
  • High resistance to stress corrosion cracking (SCC)
  • Good weldability
  • Very high strength. The proof strength is about three times as high as for conventional austenitic stainless steels.

Standards

  • UNS: S32906
  • EN Number: 1.4477

Product standards

  • Seamless tube and pipe: ASTM A789, A790
  • Bar steel: ASTM A479
  • Plate: ASTM A240

Approvals

  • Approved by the American Society of Mechanical Engineers (ASME) for use in accordance with ASME Boiler and Pressure Vessel Code, Section VIII, div. 1 and 2.
  • PED (Pressure Equipment Directive) PED 2014/68/EU and AD2000 Merkblatt W2: Particular Material Appraisal (PMA), Austenitic-ferritic steel Sandvik SAF 2906.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Send PDF via email