Sandvik 2RK65™

Tube and pipe, seamlessFolha de dados

Folha de dados atualizada 2020-01-17 16:07 (substitui todas as edições anteriores)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 2RK65™ is a high-alloy austenitic stainless steel intended for use under severe corrosive conditions within the process industry. The grade is characterized by:

  • Very good resistance to attacks in acidic environments, e.g. sulfuric, phosphoric and acetic acid
  • Very good resistance to pitting in neutral chloride-bearing solutions
  • Much better resistance to crevice corrosion than steels of the ASTM 304 and ASTM 316 types
  • Very good resistance to stress corrosion cracking
  • Good weldability

Standards

  • : '904L'
  • : N08904
  • : 4539-089-04-I
  • : 1.4539
  • : X1NiCrMoCu25-20-5

Product standards

  • ASTM A213 (seamless/welded tube)
  • ASTM A269 (seamless/welded tube)
  • ASTM A312 (seamless/welded pipe)
  • ASTM A240 (plate and sheet)
  • ASTM A276, A479, A484 (bar)
  • ASTM B677 (seamless tube and pipe)
  • EN 10216-5 (seamless tube and pipe)

Approvals

  • Approved for use in ASME Boiler and Pressure Vessel Code section VIII, div. 1 construction
  • VdTÜV-Werkstoffblatt 421 (Austenitischer Walz-und Schmiedestahl)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.