Sandvik 353 MA

Tube and pipe, seamlessFolha de dados

Folha de dados atualizada2019-08-22 07:39 (substitui todas as edições anteriores)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 353 MA is an austenitic chromium-nickel steel alloyed with nitrogen and rare earth metals. The grade is characterized by:

  • High creep strength
  • Very good resistance to isothermal and cyclic oxidation
  • Very good resistance to combustion gases
  • Very good resistance to carburization
  • Good resistance to nitriding gases
  • Good structural stability at high temperatures
  • Good weldability
  • Maximum operating temperature is approx. 1175°C (2150°F)

Standards

  • UNS: S35315
  • EN Number: 1.4854

Product standards

  • ASTM A312
  • EN 10297-2

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.