Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 3R64 is an austenitic stainless steel with a high molybdenum content. The grade is characterized by improved resistance to general and pitting corrosion in comparison with ASTM 316L.

Standards

  • ASTM: TP317L
  • UNS: S31703
  • SS: 2367

Product standards
Seamless tube and pipe

ASTM A213, A312
SS 142367

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.