Sandvik 3RE60

Tube and pipe, seamlessDatasheet

Datasheet updated 2020-12-10 07:47 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 3RE60 is a duplex (austenitic-ferritic) stainless steel characterized by the following properties:

  • High resistance to stress corrosion cracking (SCC) in chloride-bearing environments
  • Good resistance to general corrosion and pitting
  • High mechanical strength – roughly twice the proof strength of austenitic grades
  • Good resistance to erosion corrosion and corrosion fatigue
  • Physical properties that present design advantages
  • Good weldability

Standards

  • UNS: S31500
  • EN Number: 1.4424
  • EN Name: X2CrNiMoSi18-5-3
  • W.Nr.: 1.4417
  • DIN: X 2 CrNiMoSi 19 5
  • SS: 2376
  • AFNOR: Z2 CND 18.05.03

Product standards
Seamless and welded tube: ASTM A789
Seamless and welded pipe: ASTM A790
Seamless tube: EN 10216-5, NFA 49-217

Approvals
Approved for use in ASME Boiler and Pressure Vessel Code section VIII div. 1 and 2 construction NGS 1604 (Nordic rules for application of SS 2376)
VdTÜV-Werkstoffblatt 385 (Nichtrostender ferritisch-austenitischer Stahl).

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.