Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 4L7 is a carbon steel used for composite tubes.

Standards

  • ASTM: Grade A-1
  • EN Number: 1.0425
  • EN Name: P265GH
  • W.Nr.: 1.0405
  • DIN: St 45.8
  • SS: 1435

Product standards

  • ASTM A210
  • EN 10216-2
  • DIN 17175 (withdrawn)
  • SS 14 1435 (withdrawn)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.