Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 6LR62 is a molybdenum-alloyed austenitic stainless steel.

Standards

  • ASTM: TP316, TP316H
  • UNS: S31600, S31609
  • EN Number: 1.4401
  • EN Name: X5CrNiMo17-12-2
  • W.Nr.: 1.4401
  • AFNOR: Z6ZND17-12

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.