Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 7RE10 is an austenitic, stainless chromium-nickel steel of the 25/20 type, suitable for high-temperature applications. The grade is characterized by:

  • Good resistance to carburization, sulphidation, and oxidation combined with moderate creep strength and structural stability.
  • A maximum service temperature in air of 1100°C (2010°F).

Standards

  • ASTM: TP310S, TP310H
  • UNS: S31008, S31009
  • EN Number: 1.4845
  • EN Name: X 8 CrNi 25-21
  • W.Nr.: 1.4845
  • DIN: X 12 CrNi 25 21
  • SS: 2361
  • AFNOR: Z 12 CN 25.20

Product standards

Seamless tube and pipe

  • ASTM A213, A312
  • EN 10297-2
  • Stahl-Eisen-Werkstoffblatt 470
  • SS 14 23 61
  • NFA 49-117

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.