Sandvik Ti Grade 1

Tube and pipe, seamlessDatasheet

Datasheet updated 2020-12-10 06:47 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik Ti Grade 1 is an unalloyed titanium grade (CP titanium = commercially pure titanium) with low oxygen content. The grade is characterized by relatively low strength and high ductility. It is typically used for plate heat exchangers.

Standards

  • ASTM: Grade 1
  • UNS: R50250

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.