Sandvik Ti Grade 7 is an unalloyed titanium grade with standard oxygen content and addition of palladium. The grade is characterized by excellent corrosion resistance in reducing and oxidizing environments and is typically used within, for example, the chemical industries.
Standards
-
ASTM: Grade 7 -
UNS: R52400
Chemical composition (nominal)
Fe | O | C | H | N |
---|---|---|---|---|
≤0.20 | ≤0.18 | ≤0.08 | ≤0.01 | ≤0.03 |
Ti=Bal.
Pd=0.12–0.25%