Classe Sandvik UNS ASTM EN C Cr Ni Mo Outros
Programa de fabricação de barras circulares (incluindo composição química nominal)
Sanmac® 304/304L S30400/S30403 304/304L 1.4301/1.4307 ≤0.030 18.5 8.5 - -
Sanmac® 316/316L1) S31600/S31603 316/316L 1.4401/1.4404 ≤0.030 17 10.5 2.1 -
Sandvik 303 S30300 303 1.4305  <0,06 17.5  8.5  - S
Sanmac® 4435 S31600/S31603 316/316L 1.4435 ≤0.030 17.5 12.5 2.6 -
Sanmac® 4571 S31635 316Ti 1.4571 0.03 17 11 2.1  Ti
Sanmac® 22051) S31803/32205 - 1.4462  ≤0.030 22.5 5.5 3.2 N
Sanmac® 329 S32900 - 1.4460 ≤0.05 25.5 5 1.5 N
Sandvik SAF™ 25071) S32750 - 1.4410  ≤0.030 25 7 4 N
Sandvik SAF 32760 S32760 - 1.4501 ≤0.030 25 7 3.8 W, Cu, N
Sanicro® 28 N08028 - 1.4563 ≤0.020 27 31 3.5  Cu

1) A classe atende aos requisitos de PED 97/23/EC.

Barra circular do programa padrão

A barra circular inoxidável da Sandvik é entregue em comprimentos aleatórios ou cortada em comprimentos fixos. Ela é entregue com as seguintes superfícies, dependendo do tamanho:

  • Com torneamento de casca e lustrada (PTB)
  • Com torneamento de casca (PT)
  • Usinagem bruta (RM)
Diâmetro,
mm (pol.)
Tolerância,
mm (pol.)
Comprimento
aleatório, m (pé)
Peso
kg/m (lb/pé)
Sanmac
316L
Sanmac
329
Sanmac
2205
Sandvik
SAF 32760
Sandvik
SAF 2507
■ = item padrão em estoque, depósito central, □ = pode ser produzido como um pedido de fresa de Sandviken (entre em contato conosco sobre a quantidade mínima)
20.00 (0.79) -0/+0.13 (-0/+0.005) 3.5–4.5 (11.5-14.8) 2.5 (1.7)
25.00 (0.98) -0/+0.13 (-0/+0.005) 3.5–4.5 (11.5-14.8) 3.9 (2.6)
30.00 (1.18) -0/+0.13 (-0/+0.005) 3.5–4.5 (11.5-14.8) 5.5 (3.7)
35.00 (1.38) -0/+0.16 (-0/+0.006) 3.5–4.5 (11.5-14.8) 7.6 (5.1)
40.00 1.57) -0/+0.16 (-0/+0.006) 3.5–4.5 (11.5-14.8) 9.9 (6.7)
45.00 (1.77) -0/+0.16 (-0/+0.006) 3.5–4.5 (11.5-14.8) 12.5 (8.4)
50.00 (1.97) -0/+0.16 (-0/+0.006) 3.5–4.5 (11.5-14.8) 15.4 (10.3)
52.00 (2.04) -0/+0.16 (-0/+0.006) 3.5–4.5 (11.5-14.8) 17.3 (11.6) - - - -
55.00 (2.16) -0/+0.19 (-0/+0.007) 3.5–4.5 (11.5-14.8) 19.0 (12.8)
60.00 (2.36) -0/+0.19 (-0/+0.006) 3.5–4.5 (11.5-14.8) 22.2 (14.9)
61.20 (2.41) -0/+0.19 (-0/+0.006) 3.5–4.5 (11.5-14.8) 22.6 (15.2) - - - -
65.00 (2.56) -0/+0.19 (-0/+0.006) 3.5–4.5 (11.5-14.8) 26.0 (17.5)
66.20 (2.60) -0/+0.19 (-0/+0.006) 3.5–4.5 (11.5-14.8) 27.1 (18.2)
70.00 (2.76) -0/+0.19 (-0/+0.006) 3.5–4.5 (11.5-14.8) 30.2 (20.3)
71.40 (2.81) -0/+0.19 (-0/+0.006) 3.5–4.5 (11.5-14.8) 30.8 (20.7) - - - -
75.00 (2.95) -0/+1.00 (-0/+0.039) 5–7 (16.4-23.0) 34.7 (23.3)
76.40 (3.00) -0/+1.00 (-0/+0.039) 5-7 (16.4-23.0) 36 (24.2)
80.00 (3.15) -0/+1.00 (-0/+0.039) 5–7 (16.4-23.0) 39.5 (26.6)
81.40 (3.20) -0/+1.00 (-0/+0.039) 5–7 (16.4-23.0) 40.2 (27.0) - - - -
82.55 (3.25) -0/+1.00 (-0/+0.039) 5-7 (16.4-23.0) 41.9 (28.1)
85.00 (3.35) -0/+1.00 (-0/+0.039) 5–6.9  (16.4-22.6) 44.6 (30.0)
86.40 (3.40) -0/+1.00 (-0/+0.039) 5–6.9  (16.4-22.6) 45.3 (30.4) - - -
88.00 (3.46) -0/+1.00 (-0/+0.039) 5-7 (16.4-23.0) 47.7 (32.0)
90.00 (3.54) -0/+1.00 (-0/+0.039) 5–7 (16.4-23.0) 49.9 (33.5)
95.00 (3.74) -0/+1.00 (-0/+0.039) 3–7 (16.4-23.0) 55.6 (37.4)
96.40 (3.80) -0/+1.00 (-0/+0.039) 5-7 (16.4-23.0) 57.2 (38.4)
98.00 (3.86) -0/+1.00 (-0/+0.039) 5-7 (16.4-23.0) 59.2 (39.8)
100 (3.94) -0/+1.50 (-0/+0.059) 5–7 (16.4-23.0) 61.7 (41.5)
101.60 (4.00) -0/+1.50 (-0/+0.059) 5–7 (16.4-23.0) 63.6 (42.7)
102 (4.02) -0/+1.50 (-0/+0.059) 5–7 (16.4-23.0) 63.9 (43.0) - - - -
105 (4.13) -0/+1.50 (-0/+0.059) 5–7 (16.4-23.0) 68.0 (45.7)
107 (4.21) -0/+1.50 (-0/+0.059) 5-7 (16.4-23.0) 70.6 (47.4)
110 (4.33) -0/+1.50 (-0/+0.059) 5–7 (16.4-23.0) 74.6 (50.0)
112 (4.41) -0/+1.50 (-0/+0.059) 5–7 (16.4-23.0) 75.9 (51.0) - - - -
114.3 (4.50) -0/+1.50 (-0/+0.059) 5–7 (16.4-23.0) 80.5 (54.1)
115 (4.53) -0/+1.50 (-0/+0.059) 5–7 (16.4-23.0) 81.5 (54.8)
117 (4.61) -0/+1.50 (-0/+0.059) 5–7 (16.4-23.0) 82.9 (55.7) - - - -
120 (4.72) -0/+1.50 (-0/+0.059) 5–7 (16.4-23.0) 88.8 (59.8)
120.65 (4.75) -0/+1.50 (-0/+0.059) 5-7 (16.4-23.0) 89.7 (60.3)
122 (4.80) -0/+1.50 (-0/+0.059) 5-7 (16.4-23.0) 91.8 (61.7)
125 (4.92) -0/+1.50 (-0/+0.059) 5–7 (16.4-23.0) 96.3 (64.7)
127 (5.00) -0/+1.50 (-0/+0.059) 5–7 (16.4-23.0) 99.4 (66.8)
130 (5.12) -0/+1.50 (-0/+0.059) 5–7 (16.4-23.0) 104 (69.9)
132 (5.20) -0/+1.50 (-0/+0.059) 5–7 (16.4-23.0) 107 (71.7)
133.35 (5.25) -0/+1.50 (-0/+0.059) 5–7 (16.4-23.0) 110 (73.9)
135 (5.31) -0/+1.50 (-0/+0.059) 5–7 (16.4-23.0) 112 (75.3)
140 (5.51) -0/+1.50 (-0/+0.059) 5–7 (16.4-23.0) 121 (81.3)
143 (5.63) -0/+1.50 (-0/+0.059) 5–7 (16.4-23.0) 126 (84.7)
145 (5.71) -0/+1.50 (-0/+0.059) 5–7 (16.4-23.0) 130 (87.4)
150 (5.90) -0/+1.50 (-0/+0.059) 5–7 (16.4-23.0) 139 (93.4)
152.4 (6.00) -0/+1.50 (-0/+0.059) 5–7 (16.4-23.0) 143 (96.1)
153 (6.02) -0/+1.50 (-0/+0.059) 5–7 (16.4-23.0) 144 (96.8)
155 (6.10) -0/+1.50 (-0/+0.059) 5–7 (16.4-23.0) 149 (100.1)
160 (6.30) -0/+1.50 (-0/+0.059) 5–7 (16.4-23.0) 158 (106.2)
163 (6.42) -0/+1.50 (-0/+0.059) 5–7 (16.4-23.0) 164 (110.2)
165 (6.50) -0/+1.50 (-0/+0.059) 5–6 (16.4-19.7) 168 (112.9)
165.1 (6.50) -0/+1.50 (-0/+0.059) 5-6 (16.4-19.7) 168 (112.9)
170 (6.69) -0/+1.50 (-0/+0.059) 5–6 (16.4-19.7) 178 (119.6)
173 (6.81) -0/+1.50 (-0/+0.059) 5-6 (16.4-19.7) 185 (124.3)
175 (6.89) -0/+1.50 (-0/+0.059) 5–6 (16.4-19.7) 189 (127.0)
180 (7.09) -0/+1.50 (-0/+0.059) 5–6 (16.4-19.7) 200 (134.4)
184 (7.24) -0/+1.50 (-0/+0.059) 5–6 (16.4-19.7) 209 (140.4) - - - -
185 (7.28) -0/+1.50 (-0/+0.059) 5–6 (16.4-19.7) 211 (141.8) -
190 (7.48) -0/+1.50 (-0/+0.059) 5–6 (16.4-19.7) 223 (149.8) -
200 (7.87) -0/+1.50 (-0/+0.059) 5–6 (16.4-19.7) 247 (166.0) -
203.2 (8.00) -0/+1.50 (-0/+0.059) 5–6 (16.4-19.7) 255 (171.3) -
205 (8.07) -0/+1.50 (-0/+0.059) 5–6 (16.4-19.7) 260 (174.7) -
210 (8.27) -0/+1.50 (-0/+0.059) 5–6 (16.4-19.7) 272 (182.8) -
220 (8.66) -0/+1.50 (-0/+0.059) 5–6 (16.4-19.7) 298 (200.2) -
225 (8.96) -0/+1.50 (-0/+0.059) 5–6 (16.4-19.7) 312 (209.6) -
230 (9.05) -0/+1.50 (-0/+0.059) 5–6 (16.4-19.7) 326 (219.1) -
240 (9.45) -0/+1.50 (-0/+0.059) 3–6.2 (9.8-20.3) 355 (238.5) -
250 (9.84) -0/+1.50 (-0/+0.059) 3–5.9 (9.84-19.3) 385 (258.7) -
254 (10.00) -0/+1.50 (-0/+0.059) 3–5.7 (9.84-25.9) 398 (267.4) -
260 (10.24) -0/+1.50 (-0/+0.059) 3–6.9 (9.84-22.6) 417 (280.2) -
270 (10.63) -0/+1.50 (-0/+0.059) 3–5 (9.84-16.4) 450 (302.4) -
280 (11.00) -0/+1.50 (-0/+0.059) 3–7 (9.84-25.9) 483 (324.6) -
285 (11.22) -0/+1.50 (-0/+0.059) 3–5 (9.84-16.4) 501 (336.7) -
300 (11.81) -0/+2.00 (-0/+0.079) 3–5 (9.84-16.4) 555 (372.9) -
320 (12.60) -0/+2.00 (-0/+0.079) 3–5 (9.84-16.4) 631 (424.0) - -
325 (12.80) -0/+2.00 (-0/+0.079) 3–5 (9.84-16.4) 651 (437.4) - -
340 (13.39) -0/+2.00 (-0/+0.079) 3–5 (9.84-16.4) 713 (479.1) - -
350 (13.78) -0/+2.00 (-0/+0.079) 3–5 (9.84-16.4) 755 (507.3) - -
375 (14.76) -0/+3.00 (-0/+0.12) 3–5 (9.84-16.4) 867 (582.6) - -
400 (15.75) -0/+3.00 (-0/+0.12) 3–5 (9.84-16.4) 987 (663.2) - -
406.4 (16.00) -0/+3.00 (-0/+0.12) 3–5 (9.84-16.4) 1043 (701.0) - -
425 (16.73) -0/+3.00 (-0/+0.12) 3–5 (9.84-16.4) 1114 (748.6) - -
450 (17.72) -0/+3.00 (-0/+0.12) 3–5 (9.84-16.4) 1249 (839.3) - -
Padrões de barra circular*
Classe Sandvik EN 10088-3 EN 10272 AD2000-
W2/W10
ASTM A 479 ASME SA 479 NACE MR 0175
Sanmac® 316/316L 20–450 mm 20–250 mm 20–375 mm
20–450 mm 20–450 mm Independente do tamanho
Sanmac® 2205 20–450 mm 20–160 mm - 20–450 mm 20–450 mm Independente do tamanho
Sandvik® SAF 2507 20–250 mm 20–160 mm - 20–250 mm 20–250 mm Independente do tamanho

* Entre em contato conosco para obter informações sobre os padrões para classes não incluídas na tabela.