Compressor valve steel

Hardened and tempered strip steel for manufacturing many types of valves:
Compressor valves, reed valves, check valves, flapper valves, relief and relieve valves, explosion valves, diaphragms, lamellas, emergency valves, shutting and shut-off valves. They are used in, among others, the following applications:
- Air conditioning equipment
- Brake systems
- Heat pumps
- Industrial air compressors
- Refrigerators and freezers
- Vacuum pumps
Increased design freedom with our Hiflex™ compressor valve steel
Our Hiflex™ compressor valve steel enables higher valve lift, leading to increased compressor efficiency. Reduced length of valve with maintained lift enables miniaturization of the valve.
Our Hiflex™ compressor valve steel is well suited for use in compressors where higher pressures, frequencies and temperatures place increasing demands on the valve. Read more about our Hiflex™ compressor valve steel
grade | Description |
---|---|
FreeflexTM | A hardened and tempered martensitic stainless compressor valve steel alloyed with copper with excellent dimensional tolerances and flatness. |
Hiflex™ | A new generation of high-fatigue resistance stainless chromium steel giving design freedom for valves in high-frequency and high-pressure compressors. |
7C27Mo2 | A martensitic stainless chromium steel alloyed with molybdenum that has higher fatigue strength than our 20C. |
20C | A carbon steel with 1% carbon offering high fatigue strength. |
Tensile strength and thicknesses for our compressor valve steel