Sandvik 12R10 / Sandvik T302 spring wire

Wire Лист технических данных

Лист технических данных обновлен 2017-01-19 12:34 (заменены все предыдущие редакции)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 12R10 and Sandvik T302 are austenitic stainless steels characterized by moderate tensile strength, high corrosion resistance and moderate fatigue and relaxation resistance. Service temperature: -200 to 250°C (-330 to 480°F).

Standards

  • ASTM: 302
  • ISO: X9 CrNi 18-8 Grade 1 NS
  • EN Number: 1.4310 NS
  • EN Name: X 10 CrNi 18-8 NS
  • W.Nr.: 1.4310
  • JIS: SUS 302/304-WPB

Product standards

EN 10270-3
Standards not fully fullfilled
ISO 6931-1
ASTM A 313/A 313M
JIS G 4314

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.