SAF 2205™

Tube and pipe, seamlessDatablad

Datablad uppdaterat 2021-09-23 06:17 (ersätter alla tidigare versioner)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

SAF 2205™ is a duplex (austenitic-ferritic) stainless steel characterized by:

  • High resistance to stress corrosion cracking (SCC) in chloride-bearing environments
  • High resistance to stress corrosion cracking (SCC) in environments containing hydrogen sulfide
  • High resistance to general corrosion, pitting, and crevice corrosion
  • High resistance to erosion corrosion and corrosion fatigue
  • High mechanical strength - roughly twice the proof strength of austenitic stainless steel
  • Physical properties that offer design advantages
  • Good weldability

Standards

  • UNS: S31803, S32205
  • EN Number: 1.4462
  • EN Name: X2CrNiMoN 22-5-3
  • W.Nr.: 1.4462
  • DIN: X2CrNiMoN 22 5 3
  • SS: 2377
  • AFNOR: Z2.CND22.05.03

Product standards

Seamless tube:
EN 10216-5, NFA 49-217
Seamless and welded tube:
ASTM A789
Seamless and welded pipe:
ASTM A790
Flanges and valves:
ASTM A182
Fittings:
ASTM A182; A815
Plate, sheet and strip:
ASTM A240, EN 10088-2
Bar and shapes:
ASTM A276, A479, EN 10088-3 
Forged billets EN 10088-3

Approvals

  • ASME Boiler and Pressure Vessel Code, Section VIII, Div. 1 and Div. 2
  • VdTÜV-Werkstoffblatt 418 (Ferritisch-austenitischer Walz- und Schmiedestahl)
  • NACE MR0175/ISO 15156 (Petroleum and natural gas industries - Materials for use in H2S-containing Environments in oil and gas production - Part 3: Cracking-resistant CRAs (corrosion resistant alloys and other alloys) (Published:2015)
  • NACE MR0103-2012, Materials Resistant to Sulfide Stress Cracking in Corrosive Petroleum Refining Environments
  • DNV (Approval of Seamless Ferritic/Austenitic Stainless Steel Tubes and Pipes in Quality Sandvik SAF 2205)
  • ASME B31.3 Process Piping

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.