Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 8R61 is an austenitic chromium-nickel steel alloyed with molybdenum for high-temperature applications.

Standards

  • EN Number: 1.4918
  • EN Name: X6CrNiMo17-13-2
  • W.Nr.: X 6 CrNiMo 17 13
  • DIN: 1.4919

Product standards

Seamless tube and pipe:

  • EN 10216-5
  • DIN 17459

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.