Sandvik 8RE18

Tube and pipe, seamlessDatablad

Datablad uppdaterat 2019-09-04 15:10 (ersätter alla tidigare versioner)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 8RE18 is an austenitic chromium-nickel steel for high-temperature applications.

Standards

  • ASTM: TP309S, TP309H
  • UNS: S30908/S30909
  • EN Number: 1.4833

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.