Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik Zr 702 is a zirconium grade characterized by immunity to stress corrosion cracking and high resistance to pitting and crevice corrosion. The grade has very good corrosion resistance in most organic acids, excellent corrosion resistance in mineral acids, good corrosion resistance in strong alkalis and moderate mechanical strength.

Sandvik Zr 702 main characteristics:

  • High heat transfer efficiency
  • Very low thermal expansion
  • Immunity to stress corrosion cracking (SCC).
  • High resistance to localized (pitting and crevice) forms of corrosion
  • Very good corrosion resistance in most organic acids
  • Exceptional corrosion resistance in mineral acids
  • Good corrosion resistance in strong alkalis

Sandvik Zr 702 is used in environments where even the best stainless steels are not sufficiently corrosion resistant. Zirconium is in many cases the ideal choice from both technical and economical point of view (the price/life time relation).

Standards

  • UNS: R 60702

Product standards

ASTM B523 or equivalent

Approvals

ASME SB- 523 
Vd TÜV Werkstoffblatt 480 (plate specification)

Other specifications on request.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.