Sanicro® 41

Tube and pipe, seamless Datablad

Datablad uppdaterat 2018-07-05 09:25 (ersätter alla tidigare versioner)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sanicro® 41 is a nickel alloy characterized by the following properties:

  • Very good resistance to stress corrosion cracking (SCC) in chloride and sour (H2S/Cl-) environments
  • Very good resistance to corrosion in acidic media such as sulfuric acid
  • Superior resistance to pitting and crevice corrosion than steels of the ASTM 316 type
  • Good weldability

Standards

  • ASTM: Alloy 825
  • UNS: N08825
  • W.Nr.: 2.4858
  • DIN: NiCr 21 Mo

Product standards
Seamless tube and pipe, seamless heat exchanger tubes.
ASTM B163, ASTM B423

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.