Sandvik Nanoflex®

Wire Datablad

Datablad uppdaterat 2018-07-05 14:39 (ersätter alla tidigare versioner)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik Nanoflex® is a precipitation hardening stainless steel specifically designed for applications requiring high strength combined with good ductility in the final product. The grade is characterized by high formability in the as-delivered condition and its strength is increased after ageing of the final product.

The characteristics in general can be said to be a combination of properties of ordinary austenitic stainless and low alloyed ferritic steels. This means that properties such as elastic modulus, mechanical properties and thermal expansion are comparable to ferritic steels (such as low alloyed carbon steels or chromium steels) while properties such as corrosion resistance are more comparable to austenitic stainless steels.

  • Excellent mechanical properties, very high tensile strength and hardness levels can be achieved
  • Corrosion resistance comparable to ASTM 304L or ASTM 316L depending on condition
  • Retained mechanical properties at temperatures up to at least 400oC (750oF)

Standards

  • UNS: S46910

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.