Sanbar® 20 is a high strength chromium-molybdenum steel with high fatigue strength and excellent wear resistance in the as-rolled condition.

Sanbar 23 is an air-hardening, high chromium-molybdenum alloy steel with good response to surface induction hardening and suitable for carburizing. It has high fatigue strength and wear resistance in the case hardened condition.

Sanbar 61 is a high strength silicon steel with good toughness and impact resistance in the as-rolled condition.

Sanbar 64 is an air-hardening, high nickel alloy steel with good response to carburizing. It has excellent fatigue strength and wear resistance in the case hardened condition.