The Sandvik manufacturing program of billets and blooms includes a wide range of stainless steels and nickel alloys. Several grades of Sandvik stainless steel are available as Sanmac®, stainless steel with excellent machinability and consistent properties for increased cutting speeds and reduced tool wear and shorter set-up times.

Vill du veta mer?

Ring oss Mejla oss

Technical data, such as chemical composition and mechanical properties, is found in the material datasheet for the respective grade.

Sandvik grade UNS ASTM EN steel no. Billets for forging and re-rolling Extrusion billets Blooms Ingots
Round Square
Austenitic stainless steels
Sandvik 6RA11 S30300 303 1.4305
-
Sandvik 5LR11 S30400 304 1.4301
-
Sandvik 6LR11 S30400 304 1.4301
Sandvik 4LR11 S30403 304L 1.4307
-
Sandvik 3R12 S30403 304L 1.4306
Sandvik 8LR30 S32100 321/321H 1.4541
-
Sandvik 6R35 S32100 321/321H 1.4541
Sandvik 6LR62 S31600 316 1.4401
Sandvik 5R60 S31600 316 1.4436
Sandvik 4LR61 S31603 316L 1.4404
-
Sandvik 3R65 S31603 316L 1.4404
Sandvik 3R60 S31603 316L 1.4435
Sandvik 3X1R63 S31703 317L 1.4438
-
Sandvik 3R64 S31703 317L 1.4438
Sandvik 8LR70 S31635 316Ti 1.4571
-
Sandvik 5R75 S31635 316Ti 1.4571
Sandvik 7RE10 S31008 310 1.4845
Sandvik 2RK65 N08904 904L 1.4539
Sandvik 254 SMO S31254 - 1.4547
- - -
Sanmac® 304/304L S30400/
S30403
304/304L 1.4301/
1.4307
-
Sanmac® 316/316L S31600/
S31603
316/316L 1.4401/
1.4404
-
Sanmac® 1.4435 S31603 316L 1.4435
-
Sanmac® 1.4571 S31635 316Ti 1.4571
-
Sanmac® 1.4541 S32100 321 1.4541
-
Duplex stainless steels (ferritic-austenitic)
Sandvik grade UNS ASTM EN steel no. Billets for forging and re-rolling Extrusion billets Blooms
Round Square
Sandvik 5RD58 S32900 329 1.4460
-
Sandvik SAF 2304® S32304 - 1.4362
- -
Sandvik SAF 2205™ S31803 - 1.4462
Sandvik SAF 2507® S32750 - 1.4410
- -
Sanmac® 2205 S31803/
S32205
- 1.4462
-
Nickel alloys
Sandvik grade UNS ASTM EN steel no. Billets for forging and re-rolling Extrusion billets Blooms
Round Square
Sanicro® 28 N08028 - 1.4563
- -
Sanicro® 31HT N08810/
11
Alloy 800 HT 1.4959
- -
Sanicro® 32Cu N08020 Alloy 20 -
- -
Sanicro® 41Cu N08825 Alloy 825 2.4858
- -
Sanicro® 70 N06600 Alloy 600 2.4816
- -
Ferritic and martensitic steels
Sandvik grade UNS ASTM EN steel no. Billets for forging and re-rolling Extrusion billets Blooms
Round Square
Sandvik 2XC24 S41000 410 1.4006
-
Sandvik 6C27 S42000 420 1.4028
-
Sandvik 12C27 S42000 420 -
-
Sandvik 4C54 S44600 446 -
-
Sandvik 0XC34 S43000 430 1.4016
-