Gas sensors in controlled expansion alloy

Vill du veta mer?

Ring oss Mejla oss

Product description

Lightweight controlled expansion alloy carrier replacing CuW in sensor system

Application area

Sensors

CE alloy used

CE7 controlled expansion alloys

Material replaced

CuW

Advantages of using CE7 controlled expansion alloys

  • 1/6 the weight
  • Matched CTE to the GaAS chip and alumina substrate