Low-alloy steel metal powder

Sandvik's range of Osprey™ metal powder includes a wide variety of low-alloy steel metal powder. Osprey™ metal powder in low-alloy steel is used in processes, such as:

Vill du veta mer?

Ring oss Mejla oss

General steels

General low-alloy steels

Selected low-alloy steels incl. chemical composition (nominal), %
Alloy (UNS) Fe C Cr Ni Mo Si Mn S P
SCM415
(G41180)
Bal. 0.20-
0.24
0.90-
1.2
0.25 0.15-
0.30
0.15-
0.35
0.60-
0.85
0.03 0.03
4140
(G41400)
Bal. 0.38-
0.43
0.8-
1.1
-
0.15-
0.25
0.15-
0.35
0.75-
1.00
0.04 0.035
4340
(G43400)
Bal. 0.38-
0.43
0.7-
0.9
1.65-
2.00
0.2-
0.3
0.15-
0.35
0.6-
0.8
0.03 0.03
4365 Bal. 0.62-
0.66
0.7-
0.9
1.65-
2.00
0.2-
0.3
0.15-
0.30
0.6-
0.8
0.04 0.035
4605 Bal. 0.4-0.6 - 1.5-2.5 0.2-0.5 ≤1.0 - - -
8620
(G86200)
Bal. 0.18-
0.23
0.4-
0.6
0.4-
0.7
0.15-
0.25
0.15-
0.35
0.7-
0.9
0.04 0.035
SAE 52100
(G52986)
Bal. 0.98-
1.10
1.3-
1.6
-
-
0.15-
0.35
0.25-
0.45
0.025 0.025

Other low-alloy steels are also available. Contact us to discuss Sandvik's full range of metal powder alloys.

Thermal spray alloys

Low-alloy steel for thermal spray

The thermal spray powder is also suited for flame spraying or metallizing, without subsequent fusion of the coating. Good surface preparation is fundamental to the success of this process and the application of a bond coat (SB 80) is recommended.

Low-alloy steel for thermal spray, including flame spraying or metallizing incl. chemical composition (nominal), %
Alloy Description Fe C Cr Ni Si Mn Others
SC 20 Low-alloy steel Bal. 0.15 - - - 0.5 -

Other low-alloy steels for thermal spray are also available. Contact us to discuss Sandvik's full range of metal powder alloys.