Sandvik Sanergy® LT pre-coated strip steel for bipolar plates for PEM FC

Pre-coated strip steel with a thin multilayer coating for bipolar plates used in proton exchange membrane (PEM) fuel cell applications. Sandvik pre-coated strip for PEM FC is adapted to large scale production of bipolar plates. Combined with high-speed stamping or forming, the pre-coated coil provides an outstanding opportunity for the cost-effective industrial mass production of bipolar plates for PEM FC.

Vill du veta mer?

Ring oss Mejla oss

Sandvik's production of coated strip for PEM FC bipolar plates uses an advanced, environmentally friendly vacuum-coating process.

Main characteristics of Sandvik Sanergy® LT coated strip steel for PEM FC bipolar plates

  • Good interfacial contact resistance according to DoE (US Dept. of Energy) requirements (< 10 mΩ cm-2), comparable with gold or graphite
  • Corrosion in PEMFC environment < 1 µA/cm2
  • Gas-tight material
  • Low electrical degradation (less than 0.5%/1000 h)
  • Good processing and forming characteristics