Test results for Sandvik Sancrêpe crêping blades

We let a number of tissue-making companies test Sandvik Sancrêpe™ paper creping blades over a period of time. The results were outstanding, underlining the productivity gains of the Sandvik Sancrêpe™ creping blades. The table shows the lifetime improvement achieved.

Vill du veta mer?

Ring oss Mejla oss

Lifetime improvement
Tissue
machine
Machine speed,
m/min
(ft/min)
Paper weight,
g/m2
(lb)
Paper fiber
type
Sandvik
grade
Lifetime
other blades,
hours
Lifetime
Sandvik Sancrêpe blades, hours
Voith Sulzer 1070
(3530)
16-22
(10-13.5)
Virgin Sancrêpe™ RP 8 h 17 h
Andritz 1200-1500
(4000-5000)
15
(9)
Virgin Sancrêpe™ RP 7 h 11 h
Beloit 540
(1780)
40
(25)
Virgin Sancrêpe™ RP 8 h 10 h
Valmet 850-1800
(2800-2900)
17-40
(10-25)
Virgin 50% Sancrêpe™ EPS 10 h 12 h
MP 200
(660)
40
(25)
Recycled Sancrêpe™ EPS 9 h 33 h
Beloit 1030
(3400)
18
(11)
Recycled Sancrêpe™ EPS 8 h 18 h
Valmet 1280
(4200)
16.5
(10)
Recycled Sancrêpe™ EPS 10 h 17 h
Wlasna 150
(500)
36-39
(22-24)
Recycled Sancrêpe™ EPS 4 h 8 h
Valmet 1230
(4060)
20
(12)
Recycled Sancrêpe™ EPS 8 h 11 h
- 200
(660)
30-50
(18-30)
Recycled Sancrêpe™ EPS 3 h 13 h