14C28N knife steel

Ultimate combination of hardness and corrosion resistance

14C28N is the latest development in our range of knife steels. Optimized chemistry provides a top grade knife steel with a unique combination of excellent edge performance, high hardness and good corrosion resistance.

Vill du veta mer?

Ring oss Mejla oss

This new grade matches the previous highest achievable hardness without affecting the microstructure. Blade re-sharpening is therefore easy. At the same time, edge stability in terms of microchipping and edge folding or rolling is also good.

With a recommended hardness range of 55-62 HRC, 14C28N is ideal for knife applications which place very high demands on edge sharpness, edge stability and corrosion resistance such as chef's knives, pocket knives, hunting and fishing knives.

Like most of our knife steel grades, 14C28N is fineblankable enabling efficient production.

Chemical composition, % (nominal)

C Si Mn P
max
S
max
Cr N
0.62 0.2 0.6 0.025 0.010 14.0 0.11

Datasheet

14C28N