grade Width, mm (in.) Thickness, mm (in.)
Size range for our knife steels
6C27 5 - 380
(0.1968 - 14.96)
0.1 - 2.5
(0.004 - 0.098)
7C27Mo2 5 - 350
(0.1968 - 13.78)
0.1 - 4.5
(0.004 - 0.177)
12C27 10 - 380
(0.394 - 14.96)
1.00 - 4.5
(0.04 - 0.177)
12C27M 10 - 380
(0.394 - 14.96)
1.00 - 4.5
(0.04 - 0.177)
13C26 5 - 380
(0.1968 - 14.96)
0.1 - 3.0
(0.004 - 0.118)
14C28N 5 - 380
(0.1968 - 14.96)
1.00 - 4.5
(0.04 - 0.177)
19C27 5 - 340
(0.1968 - 13.38)
0.1 - 3.0
(0.004 - 0.118)