Shock absorber strip steel surfaces

Sandvik's strip steel for shock absorber shims is delivered bright, fine polished. The edges are slit and deburred. Shaved edges can be supplied on request.

Vill du veta mer?

Ring oss Mejla oss

Flatness

Maximum out-of-flatness across and along the strip is 0.30% of the nominal strip width.

Surfaces roughness

Maximum surface roughness values, cut-off 0.25 mm (0.0098 in.), are shown in the table.

Thickness
Ra
Rmax
mm
in.
μm
μin.
μm
μin.
≤0.508
≤0.020
0.10
4.0
1.0
40
>0.508
>0.020
0.25
10.0
2.5
100

Surface defects

A small number of surface defects, such as pits and roll marks, with a depth of height up to 5 μm (200 μin.) maximum is allowed. The maximum scratch depth is 2.0 μm (80 μin.).